Thursday, October 2, 2008

[MW:1181] welding to Duplex steel castings


Dear Friend,

I require details for welding practices for Welding of Duplex & super Duplex steel castings.

thanks,

sanjeev shah

--
Western Precicast Pvt.Ltd.
: Sangli Pin:416410
Maharashtra, India
Phone:+91-233-2644101, 2, 3, 2645133.
Fax:+91-233-2644612
E-Mail-  western.precicast@gmail.com

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...