Documents attached by Ragavendra and Agarwal is not disscussing about butt weld. Only about T-TS only. This is a improvement from the past (Only PT & LT) S.Senthilkumar
--- On Thu, 9/10/08, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:
From: Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> Subject: [MW:1194] RE: 1193] Re: Radiography of tube to tube sheet welds To: materials-welding@googlegroups.com Date: Thursday, 9 October, 2008, 12:30 PM
Of course we are not discussing for butt welds, any way we have conventional methods to perform RT of but welded (inner bore) tube to tube sheet joints. Infact I was looking for a good (improved) technique, equipment for the normal tube to tube sheet weld. No doubt the posting from Mr..Raghavendra and Agrawal will clear my query to some extent. I was looking for customized equipment for this type of welds. if any body has details about the manufacturers, please share Thanks! the detail shown is not applicable to examine butt welded type weld. for your info. regards, tagore
On Tue, Oct 7, 2008 at 9:23 AM, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:
-----Original Message----- From: PEMMARAJU RAGHAVENDRA [mailto:rpe@hzw.ltindia.com] Sent: Tuesday, October 07, 2008 5:30 AM To: Bathula Raghuram (Mumbai - PIPING) Subject: Re: [MW:1177] Radiography of tube to tubesheet welds
We have done extensive RT of such joints in the past. We have adopted the back radiation technique in which the source shall be moving from the front side of the joint. We have used the roli camera without guide tube and only the cranking unit wire coupled with source pigtail shall be used.The film used was of AGFA D4 with a special type of cassette with a hole at the centre.Vide this hole on the film cassette, the source enters into its position in case of back radiation technique. It is preferred to use low curie source of Ir-192 of the order 3 to 4Ci. Refer the attached word file for the source and film setup.
Instead of Gamma rays, you may use micro-focus X ray machine with hooded anode target which was developed by Sasol.
regards, RPE
Larsen & Toubro Limited www.larsentoubro.com
From: Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> Subject: [MW:1177] Radiography of tube to tubesheet welds To: "Materials-Welding (E-mail)" <materials-welding@googlegroups.com> Date: Wednesday, 1 October, 2008, 1:48 PM
Can anybody has experience with performance of RT on tube to tubesheet welds, please share details for both techniques (i.e. back radiation and forward radiation), equipment literature if any for this type RT.
Connect with friends all over the world. Get Yahoo! India Messenger. --~--~---------~--~----~------------~-------~--~----~ To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. -~----------~----~----~----~------~----~------~--~---
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
|
No comments:
Post a Comment