[MW:1186] RE: 1177] Radiography of tube to tubesheet welds

Dear Mr. Raghuram,

I have never heard or seen RT of TTS [Tube to Tubesheet joints]. TTS welds
are normally checked by Penetrant testing, Pneumatic testing and complete
penetration [during mock up tests].

I too would like to know if RT of TTS is carried out and how its done.

Thanks and regards,

Jignesh

Kuwait

For your virus protection, any attachments should be considered uncontrolled
unless they are identified in the text. The sender does not accept liability
for any virus introduced by this email or any attachment.

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Bathula Raghuram
(Mumbai - PIPING)
Sent: Wednesday, October 01, 2008 11:18 AM
To: Materials-Welding (E-mail)
Subject: [MW:1177] Radiography of tube to tubesheet welds


Can anybody has experience with performance of RT on tube to tubesheet
welds, please share details for both techniques (i.e. back radiation and
forward radiation), equipment literature if any for this type RT.


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...