Dear Sachin,

I think he requires information reqarding How HAZ will be formed during welding, What will be its crystal stractures compared to base material & weld metal, Its properties like tensile, hardness, impact campared to B/M & weld metal etc.

In total he requires welding metallurgy of welds.

regards
P.K
----- Forwarded by Kataiah/BelleliSA on 27/10/2008 04:12 م -----
"sachin sankhe" <sachin.sankhe@rediffmail.com>
Sent by: materials-welding@googlegroups.com

27/10/2008 03:04 م
Please respond to materials-welding

       
        To:        <materials-welding@googlegroups.com>
        cc:        
        Subject:        [MW:1246] Re: HAZ



 
Hi Shailesh
Your question is not clear

Regards
Sachin

On Sat, 25 Oct 2008 shailesh dave wrote :
>DEAR MEMBERS,
>
>WOULD YOU PLEASE TELL ME WHAT COULD ME THE THUMB RULE FOR HEAT AFFECTD ZONE DURING WELDING.
>
>REGARDS,
>
>S.N.DAVE
>I/C QA/QC DAS ISLAND UAE
>
>
>
>>




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...