[MW:1243] Re: 1240] Which WPS can be used

Use WPS w/o PWHT!
-----Original Message-----
From: kataiah@bilfal.com [mailto:kataiah@bilfal.com]
Sent: Monday, October 27, 2008 9:07 AM
To: Bathula Raghuram (Mumbai - PIPING)
Subject: Fw: [MW:1242] RE: 1240] Which WPS can be used


Dear Sir,

Iam not going to do PWHT  after welding.

reards

----- Forwarded by Kataiah/BelleliSA on 27/10/2008 11:05 ص -----
"Bathula Raghuram \(Mumbai - PIPING\)" <R.Bathula@ticb.com>
Sent by: materials-welding@googlegroups.com

27/10/2008 10:47 ص
Please respond to materials-welding

       
        To:        <materials-welding@googlegroups.com>
        cc:        
        Subject:        [MW:1242] RE: 1240] Which WPS can be used



it depends on after treatment of this weld, is this weld required or subjected to PWHT?
-----Original Message-----
From:
materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com]On Behalf Of kataiah@bilfal.com
Sent:
Sunday, October 26, 2008 9:38 AM
To:
materials-welding@googlegroups.com
Subject:
[MW:1240] Which WPS can be used


Dear Frinds ,


I have a requirement to weld  Stress relievedCS  plate # normal CS Plate.


Which WPS can is use to weld such combination ( i mean a WPS with PWHT or with out PWHT).


ASME is refering anywhere which type to be used?


What is the logic to use perticular type?.


Regards


P.K.

Bilfal Industries.
 



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...