Double welded groove welds are considered welding with backing, refer QW 402.4
-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com]On Behalf Of Hardik Desai
Sent: Saturday, October 18, 2008 8:24 PM
To: materials-welding@googlegroups.com
Subject: [MW:1221] For Welder
Dear sirs,One welder is qualified with Backing for SMAW process.One welder is doing welding for Single V Butt Joint with 2-3 gap. backgouging is applicable. After SMAW three run, Other run by other welder with FCAW process. After Backgouging Other side welding by FCAW process.Now my question is First welder is done SMAW with 2-3 gap without backing it is acceptable or not?I hope for your reply.Thanks & Regards
--~--~---------~--~----~------------~-------~--~----~
CONFIDENTIALITY NOTICE
This e-mail and any attachments there to contain information, which is confidential, proprietary, privileged and/or protected from disclosure by intellectual property rights and are intended for the sole use of the recipient(s) named above. If you are not the intended recipient of this message you are hereby notified that any dissemination or copying of this message is strictly prohibited. If you have received this e-mail in error, please notify the sender either by telephone or by e-mail and delete it from any computer. Although this e-mail and any attachments thereto are believed to be free from any virus or other defects, which might affect any computer or IT system, it is the responsibility of the recipient to ensure that they are virus free. We are not liable for any loss or damage arising in any way from receipt or use there of. Thank you.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---