Monday, October 27, 2008

[MW:1246] Re: HAZ

 
Hi Shailesh
Your question is not clear

Regards
Sachin

On Sat, 25 Oct 2008 shailesh dave wrote :
>DEAR MEMBERS,
>
>WOULD YOU PLEASE TELL ME WHAT COULD ME THE THUMB RULE FOR HEAT AFFECTD ZONE DURING WELDING.
>
>REGARDS,
>
>S.N.DAVE
>I/C QA/QC DAS ISLAND UAE
>
>
>
>>



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...