[MW:1137] Re: FW: Propane sphere collapse

Sirs,

Can you please mail the original mail on this topic. The same was deleted from our computer by mistake.

Thanks & Regards,

G. A. Soman
PRINCIPAL
DON BOSCO MARITIME ACADEMY,
Premier automobiles Road,
Kurla West, Mumbai 400 070
Tel: 022 - 2504 1585 / 2018

----- Original Message -----
From: Ron Mays <ronm-mec@nmit.vic.edu.au>
Date: Thursday, September 18, 2008 12:21 pm
Subject: [MW:1133] Re: FW: Propane sphere collapse
To: "Materials-Welding (E-mail)" <materials-welding@googlegroups.com>

> Thank you Sohil, I think this is a good lesson for all my students.
>
>
> Ron Mays
>
> (03) 9269 8661 wk.
> 0417 354 108 mob.
> (03) 9269 8673 fax.
>
> >>> "Bathula Raghuram (Mumbai - PIPING)" <R.Bathula@ticb.com>
> 17/09/2008 5:51 pm >>>
>
> sharing info...
>
> From: Vyas, Sohil U. - EHES HSE (HAZ)
> Sent: Wednesday, September 17, 2008 9:02 AM
> To: Acharya, Darpan T. - EHES Ref. Equip - Planning (HAZ); Gor,
> Dharmesh C - EHES Ref. Equip - Production (HAZ); Patel,
> Parimalkumar C - ECIL Production (HAZ); Parmar, Bhavesh B - EHES
> Production (HAZ); Sisodiya, Manoj K. - EHES Ref. Equip - Production
> (HAZ); Patel, Mitesh J. - EHES Electrical (HAZ); Patel, Ashish K -
> EHES Electrical (HAZ); Kelawala, Pranav N - EESL DRI Group (HAZ);
> Gandhi, Ashish H. - EHES Ref. Equip - Production (HAZ); Varia,
> Narendra R - EHES Production (HAZ); Sahu, Suresh K - EHES
> Production (HAZ); Shah, Mayur S - EHES Production (HAZ); Mohammad
> M. Alam - EHES Steel & MH Equip - Production (HAZ); Patel, Rajesh D
> .- ECIL Safety (HAZ); Bhatt, Chirag J - EHES Administration (HAZ);
> Lainingwala, Rinky P - EHES Administration (HAZ)
> Cc: Sarin, Ravi - EHES (HAZ); Chakravarty, Gautam - EHES Ref. Equip
> (HAZ); Krishnan, Udaykumar - EHES Steel & MH Equip (HAZ); Singh,
> Tarwendar - EHES Production (HAZ); Swaminathan, Sridhar - EHES
> Stores (HAZ); Lokeshkumar, L. - EHES Electrical (HAZ); Tulsi, Capt
> Rupinder - EHES Administration (HAZ)
> Subject: Propane sphere collapse
> Respected All, Please look at the attached of incident occurred
> during hydro test, its lesson for learning. Regards,Sohil U.
> VyasSafety - EHES (E C I L)Mo. : + 91 98792 02751email :
> Sohil.Vyas@essar.com(We serve to Save)
>
>
> _____________________________________________________________________
> This e-mail has been scanned for viruses by MCI's Internet Managed
> Scanning Services - powered by MessageLabs. For further information
> visit http://www.mci.com
>
>
>
>
> _____________________________________________________________________
> This e-mail has been scanned for viruses by MCI's Internet Managed
> Scanning Services - powered by MessageLabs. For further information
> visit http://www.mci.com
> >
>

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...