Dear All,
 
Can you suggest any suitable welding consumable for Pipes and welding fittings of material: St. 35.8 DIN 2448 with 3.1B certificate.

 

Regards
Sharif
BOC Bangladesh Limited.


 
On 9/18/08, Bagesh Kumar <bagesh.kmr@gmail.com> wrote:

 

Dear All,
The Fluid for Industrial Heating Water is a mixture of Glycol 56 % and Water 44 %,

PMC has suggested use of Low Temperature Carbon Steel Materials,

Please Throw some light on  Proper Piping Material for the said Fluid, The Design Temperature is 130 Deg C Max and Pressure is 16 Kg/Cm2.
I have used previously SS 316, For MEG Service, Services in a petrochemical plant.

Kumar Bagesh

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...