[MW:1102] Test Coupon - Mild Steel Plate

What will be the dimensions for a mild steel plate test coupon, welded using MMWA in all positions or only 6G position to qualify a welder?

 

NIALEL LUKAS

Mechanical Engineering

PO Box 104, Lihir,NIP 

PH: 986 5360

FAX: 968 5359

 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS