Wednesday, September 10, 2008

[MW:1091] Fabricating 350 x 300 Reducer


MMWA can be used to fabricate such miter reducers, however an additional thing to be noted is that it is not in acc. with B31.3 which is also applicable for geothermal piping. And should be designed as per ASME sec 8. Also 31.3 para 304.6 to be noted on reducers.

With regards,
Kannan




<Nialel.Lukas@lglgold.com>
Sent by: materials-welding@googlegroups.com

06/09/2008 22:36

Please respond to
materials-welding@googlegroups.com

To
<materials-welding@googlegroups.com>
cc
Subject
[MW:1085] Fabricating 350 x 300 Reducer





Hi,
 
Is it possible to fabricate a 350 x 300 reducer from Pipe, ASTM 106, Sch XS, manually using MMWA, All position welding, and use it on Geothermal Piping of Steam? The live steam temperature is 158 deg.Celcius in the pipe and discharges at 100 deg. Celsius. Can anyone explain why it is not so or can be used?
 
Thank you,
 
NIALEL LUKAS --~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...