Saturday, September 13, 2008

[MW:1112] Re: Cold Bending of SS.304 1.1/2" size pipe / tube

Refer to Clause  RCB-2.31. It restarins to 17% thinning  for work hardened materials. It also refers to 2.33 on HT.
In industry practice, Austenetic SS materials are considered to be of  work hardening type and  the above clauise ais applied for Heat Exchnager tubes.
Tagore 

 
On 9/11/08, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:
You may use Table UHA44 (ASME Sec VIII div1) for PFHT requirement, which is most common in HE  U tubing.
Para 331.4.2 not clearly spelt out for P8 material, but there is something called 10% strain limit, which is same as given in UHA44 for 304 material
 
 
From Dhwani Desai........

desaid@toyoindia.com

11/09/2008 03:53

To
Kannan.Sundaram@Linde-LE.com
cc
Subject
Cold Bending of SS.304 1.1/2" size pipe / tube


Hi,

Is there any code restriction for doing cold bending of SS-304 (1.1/2") pipe? Any post bending heat treatment required?
31.3 only specifies heat treatment for ferritic steel.


thanks & Regards,

Dhwani
 
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...