[MW:1175] TKY Joints defination and use of 6GR Welders

AWS D1.1/D1.1M :2006 para 2.24.1.5 (2) , attached, states that classification criteria of TKY joints is based on punching load cases of brace to chord connection.

Now the question is that:

The given weld connection is tubular to tubular (TKY type) but does not fall under TKY classification based on punching load cases as para 2.24.1.5.
for example secondary and miscellaneous small structures like access platforms , stairs  etc fabricated by tubulars/ pipes.
Do we need to treat these tubular to tubular joints as TKY joints and strictly welded by 6GR qualified welders??


--
Thanks

Vinod R Upadhyay
SMOE (a subsidiary of SEMBCORP MARINE)
Batam Yard, QA/QC- TOTAL Project
Mob:+62 815 1474 1550



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...