[MW:1127] Re: MS & SS welding

 
There is absolutely no problem in welding mild steel plates with
>SS304 plates. They are welded with E 309L electrodes.

Regards
Prem S Nautiyal


On Wed, 17 Sep 2008 dev yadav wrote :
>Dear All,
>
>Please suggest, is there any problem in welding of mild steel plates with
>SS304 plates.
>
>--
>DEVENDRA KUMAR YADAV
>Design Engineer
>Lars Enviro Pvt. Ltd.
>
>>

PREM S NAUTIYAL
CELL : 9820313278

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...

Ebay

Pages

Contributors

Blog Archive