Excuse me.

Ok,  i suggest use interpass temperature of  300 degrees Farenheit.



carlos oliveros

On Wed 17/09/08 09:42 , "PREM SHANKARDUTT NAUTIYAL" prem_nautiyal@rediffmail.com sent:

  I suggest you use interpass temperature of 150 degrees celcius max. while welding.

Regards

Prem Nautiyal


On Wed, 17 Sep 2008 carlos oliveros wrote :
>  BODY { font-family:Arial, Helvetica, sans-serif;font-size:12px; } Is
>not Problems if you applicate the correct electrode (E-309) and
>interpass controlled 300 degree Max
>  carlos oliveros
>  On Wed 17/09/08 09:15 , "dev yadav" devendrayadav09@gmail.com sent:
>    Dear All,
>  Please suggest, is there any problem in welding of mild steel plates
>with SS304 plates.
>
>  --
>  DEVENDRA KUMAR YADAV
>  Design Engineer
>  Lars Enviro Pvt. Ltd.
>
>>

PREM S NAUTIYAL
CELL : 9820313278



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...

Ebay

Pages

Contributors

Blog Archive