No problem.Use AWS E309-16 class electrodes for SMAW process and ER309 Filler wire for GTAW process.
Rgds
Aarpee

 
On 9/17/08, dev yadav <devendrayadav09@gmail.com> wrote:
Dear All,

Please suggest, is there any problem in welding of mild steel plates with SS304 plates.

--
DEVENDRA KUMAR YADAV
Design Engineer
Lars Enviro Pvt. Ltd.

 
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...