If contract doc. doesn't say and the PMC suggests a diff material, you/your process dept. have to weight the overall cost saving solution and make the decision.
Either to use SS and no inhibitor (or) LTCS with inhibitor.

In case if you are interested to know about tomsol just search in the net for 'Tomsol MSDS' . In case if you are not aware of MSDS, it is the abbreviation of 'Material Safety Data Sheet' which gives more info on the chemical.

With regards,
Kannan



"Bagesh Kumar" <bagesh.kmr@gmail.com>
Sent by: materials-welding@googlegroups.com

18/09/2008 13:13

Please respond to
materials-welding@googlegroups.com

To
"'Desai Jignesh \(Mumbai - Piping\)'" <J.J.Desai@ticb.com>
cc
<materials-welding@googlegroups.com>
Subject
[MW:1144] RE: 1132] Piping Materials for Hot water Tracings.





 
The Contract document does not specify any additive inhibiters in Glycol present, I believe that LTCS Materials can be used but without additive inhibitors the Acid formation will be there which will be highly risky.
 
I think Tomsol A 40 or A 65 additives used as inhibitors element in Glycol to prevent Acid formation. But still not clear about this process data.

Kumar Bagesh



From: Desai Jignesh (Mumbai - Piping) [mailto:J.J.Desai@ticb.com]
Sent:
Thursday, September 18, 2008 7:43 PM
To:
bagesh.kmr@gmail.com
Subject:
FW: 1132] Piping Materials for Hot water Tracings.

 
Bhagesh
 
FYI, we have used LTCS and CS material for Glycol water service in Borouge II project.
Now I do not have process dat with me.
 
Regds/Jignesh --~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...