[MW:1089] Re: flash butt welding

AWS D1.1 standard and base material is ASTM 1011 Gr 36

On Aug 28, 7:45 pm, Raghuram Bathula <raghurambath...@gmail.com>
wrote:
> what code your are using and what is your material?
>
> On 28 Aug, 19:41, mgk <mgkuma...@gmail.com> wrote:
>
> > can any one tell what are the essential variables which we have to
> > consider when we are welding plate thickness of 8 and 12 mm by flash
> > butt welding

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...