I think you are looking for weld overlay on P1 by P8
please let me know which process you are doing ESW or GTAW or SMAW
as far as Strip cladding is concerend i think Soudotape is the only
genuine supplier in htis categorry.
as far as AWS class i will mail you later.
bye
On Jul 26, 5:14 pm, Romio <romiomda...@gmail.com> wrote:
> Has anybody experienced UNS31254 (P No. 8 Gr. 4.....chemi..20Cr 18Ni
> 6Mo) weldoverlay on SA516 Gr. 70
> Can someone suggest the correct AWS class? If u can suggest the STRIP
> consumable supplier for the smae it will be handful....
>
> Romio
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Comments