Reduced rating is common where a conservative approach is applied in defining the piping materials while shaping the piping material classes.
Conservative... in the context of reduced thickness of pipes and fittings and having in some cases a reduced pressure rating of flanges. Subjectively, handling such cases is a little bit complex due to the nature of broad aspect of the parameters involved.

In a process plant, there will be few border cases of design conditions in the process streams, by which I mean the borders of the ANSI B16.5/B16.34 rating tables. On certain cases reducing to the next lower pressure rating will benefit a turnkey contractor, considering down the line cost benefit depending upon the quantum of piping involved in those streams. During such cases the piping material engineer who optimizes the PMC-piping material class concludes with process engineer to reduce the design condition.

In these border cases there are two aspects.
1) The simple safety factor reduction of the process condition judged by the process engineer.
2) The process stream may not be subjected to the defined design condition continuously, but on a cyclic or only for a short period of duration. ANSI B31.3 / 1 allows such temporary surging under certain criteria (Refer the code for details). Under such limitations, the piping material engineer works/designs the PMC with reduced pressure rating conditions also called as a STC - short term condition.

So in conclusion such conservative approach helps in avoiding Over Designing the piping system with the ANSI code as an excuse/backing. Addtionally, such concept has significance when the quantum of piping is extremely high and if the streams are in higher temp. ranges where material selection plays a very important role.

With regards,
Kannan




"Bathula Raghuram \(Mumbai - PIPING\)" <r.bathula@ticb.com>
Sent by: piping_valves@yahoogroups.com

17/07/2008 13:29

Please respond to
piping_valves@yahoogroups.com

To
<materials-welding@googlegroups.com>
cc
<piping_valves@yahoogroups.com>
Subject
[piping_valves] RE: 941] Flange Reduced Rating





Can you please elaborate!

Is it something related to DIN flanges? I don’t know exactly but probably the P/T ratings are reduced while revising the new EN standards (PrEN1092?) for PN based flanges.

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Hari Srinivasa Murthy
Sent:
Thursday, July 17, 2008 4:25 PM
To:
materials-welding@googlegroups.com
Subject:
[MW:941] Flange Reduced Rating

 


Dear Sh. Raghuram/Member of materials group,

 

Can you please explain about " Flange Reduced Ratings".

 

Regards

 

Srinivasa Murthy

__,_._,___
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...