Dear Zameer
 
As per sec VIII u can welld over weld. dont worry u can weld ir , but do 100% MPI or DP
 
Regards
 
Shabbir

 
On 7/13/08, Zameer Mohammed <dreamthinkwork@gmail.com> wrote:

Dear Friends,

We have to weld a Baffle plate of 10mm Thick inside an EQ. TEE (24'', 36'' & 42''). The thickness of the TEE is 9.53 mm and all the EQ. TEES are welded construction with 100% RT. The Baffle plate is welded in such a way that, it will block the one run side of the EQ. TEE. Now the welding of the Baffle plate, will it creates and problem as it intersect with EQ. TEE weld at some point. Can we have two welding at a same point? The Baffle plate is fillet welded. The working pressure is 1 bar.

Kindly advice me,

Thank you,

Regards,

 

Sabir

 

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...