25CrMo4 (1.7218) as per EN10083-3

SCM 430 as per JIS G4053 (not 430H, recheck? Or may be 425/435H?)

AISI4130

Are mostly similar in chemistry with 1Cr and 0.15-0.3Mo

No idea about SIS 2225


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of sachin sankhe
Sent: Tuesday, July 22, 2008 6:46 PM
To: materials-welding@googlegroups.com
Subject: [MW:959] Chemical/Mechanical property

 
Dear Friends,

Request you to send me chemical/Mechanical properties of undermentioned material

1.25Cr Mo4 as per EN10083-1

 


2.SCM 430H as per JIS Standard

3.SIS 2225 as per Swedish standard.
All these material are equivalent to AISI 4130.

Also request if any body can send EN10083-1/2  (such requests are not entertained in this group, neither ask for any copyright material.)
Regards
Sachin.Sankhe


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...