Dear Friends,
We have to weld a Baffle plate of 10mm Thick inside an EQ. TEE (24'', 36'' & 42''). The thickness of the TEE is 9.53 mm and all the EQ. TEES are welded construction with 100% RT. The Baffle plate is welded in such a way that, it will block the one run side of the EQ. TEE. Now the welding of the Baffle plate, will it creates and problem as it intersect with EQ. TEE weld at some point. Can we have two welding at a same point? The Baffle plate is fillet welded. The working pressure is 1 bar.
Kindly advice me,
Thank you,
Regards,
Sabir
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Monday, July 14, 2008
[MW:914] Re: Welding Baffle Plate on EQ. TEE
Request you to elaborate the problem, It seems that this Baffle plate which you are going to weld is intersecting with the flow of the fluid also.
On 7/13/08, Zameer Mohammed <dreamthinkwork@gmail.com> wrote:
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-