Keep 2.5 mm to 3.2 mm root gap.

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Bathula Anil
Kumar
Sent: 22 June, 2008 1:47 AM
To: materials-welding@googlegroups.com
Subject: [MW:880] clarification reg root gap

Dear Friends,

My Name is Anil Kumar working as a Quality Control Inspector in Qatar,
for Decon for an Oil Refinery project. I Joined the company recently and
during my regular visits to site and also reviewing various data sheets
I found that most of the defects are Root undercut, LOP and LOF, the
welding used for the production is TIG welding with 2.4mm filler wires
for all SS, CS and LTCS materials the Dia of the pipes ranges from 2inch
to 24 inch and yeah there is lot of problem with the material reg the
mismatch and ovality in the pipe apart from this another prob I observe
that the root gap used for the welding is mostly 4+ mm for all the
joints , I strongly recommended for 2.5 to 3.5 mm at the max for the
Root gap but some of the welders complaining that they are finding
difficulty in moving the electrode.

I request you to kindly suggest me what is the root gap for the above
said materials and what are the other possibilities for the above said
repairs and the corrective action required to be taken for the same.

I thank you one and all very much for creating such a beautiful group

Thanking you,

Regards

Bathula Anil Kumar

Visakhapatnam


________________________________

From Chandigarh to Chennai - find friends all over India. Click here.
<http://in.rd.yahoo.com/tagline_groups_10/*http://in.promos..yahoo.com/g
roups/citygroups/>

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...