[MW:952] RE: 950] RE: 948] Re: why CC2235-9 is not applicable for ASME Sec.III

Acceptance criteria does not change as per flaw location or direction. The acceptance criteria is based on size of flaw as per code case.

 

Regards,

Rohit Bafna

Director - Global Sales

 

------------------------------------------

TCR Engineering Services (India)
TCR Arabia (KSA), TCR Kuwait

TCR World Inc. (USA)

USA Tel: +1-240-505-0739

India Tel: +91-983-353-0400

www.tcreng.com
Material Testing | Consulting | Inspection | NDT Services

-------------------------------------------

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Bathula Raghuram (Mumbai - PIPING)
Sent: Monday, July 21, 2008 12:59 AM
To: materials-welding@googlegroups.com
Subject: [MW:950] RE: 948] Re: why CC2235-9 is not applicable for ASME Sec.III

 

In my opinion neither code nor CC distinguishes the diff. between flaw direction longitudinal/transverse (please correct me I am a level zero in UT), hence your interpretation could be correct.

However Fig2 of CC shows something transverse and longitudinal planar flaws (could we interpret like that?)

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of raghavendra pemmaraju
Sent: Saturday, July 19, 2008 7:52 PM
To: materials-welding@googlegroups.com
Subject: [MW:948] Re: why CC2235-9 is not applicable for ASME Sec.III

 

Dear All,

One more query, this time related to acceptance criteria as per ASME CodeCase 2235-9.

For the flaws oriented transverse to weld centre line axis, what is the acceptance criteria as per above CC.

As per me the above CC is silent on this and hence we need to apply the same acceptance criteria as mentioned in tables 1,2 &3 of above CC. What is your opinion.!!!!

 

regards,

Raghavendra

 
--- On Wed, 7/16/08, raghavendra pemmaraju <pemma_raghav@yahoo.com> wrote:

From: raghavendra pemmaraju <pemma_raghav@yahoo.com>
Subject: [MW:931] why CC2235-9 is not applicable for ASME Sec.III
To: materials-welding@googlegroups.com
Date: Wednesday, July 16, 2008, 10:28 PM

We are aware that ASME code case 2235-9 is appliabcle for ASME Sec.I,Sec.VIII and Sec.XII. Why not the same is applicable incase of ASME Sec.III. Where as if we see the philosophy of the above CodeCase is mainly drawn from the nuclear code ASME Sec.XI at the same time.

Can any one comment on the above.

 

regards,

Raghavendra

ASNT Level III ( RT,UT & MT) & RSO L-III

Manager,QC

L&T Ltd., Hazira

Surat

 

 


 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...