[MW:895] RE: 893] pre heat for dissimilar metals

Pre heat only on CS side


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Muhammed Ibrahim
Sent: Thursday, July 03, 2008 7:14 PM
To: materials-welding@googlegroups.com
Subject: [MW:893] pre heat for dissimilar metals

 

Any body can help me to decide the pre heat temperature for welding of carbonsteel with stainless steel?  If thickness is greater than 32mm,  preheat is mandatory in SEC VIII. But in this case what I can follow. Carbon steel preheat temperature or stainless steel preheat temperature?.

If it damage the property of stainless steel is it mandatory?

Thanks & Regards
Muhammed Ibrahim PK


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...