Dear Raghvendra,
SNT TC 1A is recommended practice for the employer for the qualification & Certification of their NDT personel.
CP 189 is ASNT standard.
Level III Requirement:
As per SNT TC 1A - Any person nominated by Employer can be LEVEL III for his company.
                          
CP 189- ASNT NDT LEVEL III is must.
 
SNT TC is much liberal for the employer and employer can set the system suitable for him. But that will not be accepted by each and every client.
 
So better to follow CP189 for the NDT personnel qualification requirements. So at least one standardisation will be there and system will be more valuable when you are presenting to your Client.
 
Regards,
Nilesh Pathare.
TCR Engineering Services, Mumbai

 
On Wed, Jul 2, 2008 at 2:25 AM, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:


I would like to know why you need two different documents (off course
one is a standard and the other is a recommended practice)

 -----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of RAGHAVENDRA
PEMMARAJU
Sent: Wednesday, July 02, 2008 10:47 AM
To: materials-welding@googlegroups.com
Subject: [MW:885] comparision between CP189 and Snt-TC-1A ( 2001
editoins)


Dear Group  members,
Could any one of you pl.provide the comparision of the above two
documents if already worked out!


regards,
Raghavendra

Larsen & Toubro Limited
www.larsentoubro.com


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...