Skip to main content

List of national European Steel Standards corresponding to EURONORM

Corresponding National Standards in
EURONORM Germany France United Kingdom Spain Italy
17 DIN 59110 NF A 45-051

---

UNE 36-089 UNI 5598
18 --- NF A 03-111

BS 4360

UNE 36-300 UNI-EU 18
UNE 36-400
19 DIN 1025 T5 NF A 45-205

---

UNE 36-526 UNI 5398
24 DIN 1025 T1 NF A 45-210

BS 4

UNE 36-521 UNI 5679
DIN 1026 UNE 36-522 UNI 5680
53 DIN 1025 T2 NF A 45-201 BS 4 UNE 36-527 UNI 5397
DIN 1025 T3 UNE 36-528
DIN 1025 T4 UNE 36-529
54 DIN 1026 NF A 45-007 BS 4 UNE 36-525 UNI-EU 54
56 DIN 1028 NF A 45-009 1) BS 4848 UNE 36-531 UNI-EU 56
57 DIN 1029 NF A 45-010 1) BS 4848 UNE 36-532 UNI-EU 57
58 DIN 1017 T1 NF A 45-005 1) BS 4360 UNE 36-543 UNI-EU 58
59 DIN 1014 T1 NF A 45-004 1) BS 4360 UNE 36-542 UNI-EU 59
60 DIN 1013 T1 NF A 45-003 1) BS 4360 UNE 36-541 UNI-EU 60
61 DIN 1015 NF A 45-006 1) BS 970 UNE 36-547 UNI 7061
65 DIN 59 130 NF A 45-075 1) BS 3111 UNE 36-546 UNI 7356
66 DIN 1018 --- --- --- UNI 6630
91 DIN 59 200 NF A 46-012 BS 4360 --- UNI-EU 91
103 DIN 50 601 NF A 04-102 BS 4490 UNE 7-280 ---
162 DIN 17 118 NF A 37-101 BS 2994 UNE 36-570 UNI 7344
DIN 59 413
168 --- NF A 03-116 BS 4360 UNE 36-800 UNI-EU 168
CECA IC 2 SEW 088 NF A 36-000 BS 5135 --- ---
1) To add NF A 45-001 and NF A 45-101 for the tolerances.

Corresponding National Standards in
EURONORM Belgium Portugal Sweden Austria Norway
17 NBN 524 NP 330

---

--- ---
18 NBN A 03-001 NP 2451

SS 11 01 20

--- NS 10 005

SS 11 01 05

19 NBN 533 NP 2116

SS 21 27 40

M 3262
24 NBN 632-01 ---

SS 21 27 25

M 3261 NS 911
SS 21 27 35
53 NBN 633 NP 2117 SS 21 27 50 --- NS 1907
SS 21 27 51 NS 1908
SS 21 27 52
54 NBN A 24-204 NP 338 --- M 3260 ---
56 NBN A 24-201 NP 335 SS 21 27 11 M 3246 NS 1903
57 NBN A 24-202 NP 336 SS 21 27 11 M 3247 NS 1904
58 NBN A 34-201 --- SS 21 21 50 M 3230 NS 1902
59 NBN A 34-202 NP 333 SS 21 27 25 M 3226 NS 1901
NP 334
60 NBN A 34-203 NP 331 SS 21 25 02 M 3221 NS 1900
61 NBN A 34-204 --- --- M 3227 ---
65 NBN A 24-206 --- --- M 3223 ---
66 --- --- --- --- ---
91 NBN A 43-301 --- SS 21 21 50 M 3221 ---
103 NBN A 43-301 --- SS 21 21 50 M 3221 ---
162 NBN A 14-101 NP 1787 --- --- ---
168 --- --- SS 11 00 12 --- ---
CECA IC 2 --- --- SS 06 40 25 --- ---
Data from www.mesteel.com

EURONORM + Corresponding national Steel standards
Designation Corresponding old designations in

According to EN 10027-1 and ECISS IC 10

According to EN 10027-2 According to EN 10025:1990 Germany France United Kingdom Spain Italy Belgium Sweden Portugal Austria Norway
S185 1.0035 Fe 310-0 St 33 A 33 A 310-0 Fe 320 A 320 13 00-00 Fe 310-0 St 320
S235JR 1.0037 Fe 360 B St 37-2 E 24-2 Fe 360 B AE 235-B 13 11-00 Fe 360-B NS 12 120
S235JRG1 1.0036 Fe 360 BFU USt 37-2 - - - AE 235 B-FU USt 360 B NS 12 122
S235JRG2 1.0038 Fe 360 BFN RSt 37-2 - - - 40 B AE 235 B-FN 13-12-00 RSt 360 B NS 12 123
S235J0 1.0114 Fe 360 C St 37-3 U E 24-3 40 C AE 235 C Fe 360 C AE 235-C Fe 360 C St 360 C NS 12 124
St 360 CE
S235J2G3 1.0116 Fe 360 D1 St 37-3 N E 24-4 40 D AE 235 D Fe 360 D AE 235-D Fe 360 D St 360 D NS 12 124
S235J2G4 1.0117 Fe 360 D2 - - -
S275JR 1.0044 Fe 430 B St 44-2 E 28-2 43 B AE 275 B Fe 430B AE 255-B 14 12-00 Fe 430 B St 430 B NS 12 142
S275J0 1.0143 Fe 430 C St 44-3 U E 28-3 43 C AE 275 C Fe 430 C AE 255-C Fe 430C St 430 C NS 12 143
St 430 CE
S275J2G3 1.0144 Fe 430 D1 St 44-3N E 28-4 43 D AE 275 D Fe 430 D AE 255-D 14 14-00 Fe 430 D St 430 D NS 12 143
S275J2G4 1.0145 Fe 430 D2 - - - 14 14-01
S355JR 1.0045 Fe 510 B - - - E 36-2 50 B AE 355 D Fe 510 B AE 355-B Fe 510 B
S355J0 1.0553 Fe 510 C St 52-3 U E 36-3 50 C AE 355 C Fe 510 C AE 355-C Fe 510 C St 510 C NS 12 153
S355J2G3 1.057 Fe 510 D1 St 52-3 N 50 D AE 355 D Fe 510 D AE 355-D Fe 510 D St 510 D NS 12 153
S355J2G4 1.0577 Fe 510 D2 - - -
S355K2G3 1.0595 Fe 510 DD1 - - - E 36-4 50 DD AE 355-DD Fe 510 DD
S355K2G4 1.0596 Fe 510 DD2 - - - - - -
E295 1.005 Fe 490-2 St 50-2 A 50-2 A 490 Fe 480 A 490-2 15 50-00 Fe 490-2 St 490
15 50-01
E335 1.006 Fe 590-2 St 60-2 A 60-2 A 590 Fe 580 A 590-2 16-50-00 Fe 590-2 St 590
16 50-01
E360 1.070 Fe 690-2 St 70-2 A 70-2 A 690 Fe 680 A 690-2 16 55-00 Fe 690-2 St 690
16 55-01
Data from www.mesteel.com Source: http://mdmetric.com

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...