[MW:545] Re: Hydrotesting of Bellow Seal Valves


Shwani,

Hydrotest of bellow seal valve is carried out with bellows installed. The manufacturer do the low pressure air testing internally to ensure the welds in bellows are free from any leakage. Then the hydrotest of complete body including bellows will be undertaken. The valve is kept open and the bellows will be subject to external pressure.

When conducting the seat closure test the bellow will not see the pressure.
 

Best Regards,

Sanjay Gandhi



desaid@toyoindia.com
Sent by: materials-welding@googlegroups.com

31/01/2008 12:29 PM

Please respond to
materials-welding@googlegroups.com

To
piping_valves@yahoogroups.com
cc
materials-welding@googlegroups.com
Subject
[MW:542] Hydrotesting of Bellow Seal Valves





Dears,


Can any one inform how testing (hydro & pneumatic) of Bellow seal valves are generally carried out? Shell Test & seat test both.

i.e. with bellows or without bellows?


If there is some detailed procedure available of reputed vendor then pls. send.


Thanks & Regards,

Dhwani Desai.

======================================================= Confidentiality Notice  This communication and the information it contains:-  (a) Is intended for the person(s) or organisation(s) named above and for no other person(s) or organisation(s).   (b) May be confidential, legally privileged and protected in law. Unauthorised use, copying or disclosure of any of it may be unlawful. If you have received this communication in error, please contact us immediately by email at Postmaster@fwuk.fwc.com. ======================================================= 
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...