Wednesday, July 21, 2010

[MW:6054] 15 NiCuMoNb 5/1.6368 (WB36)

 

 

Dear all,

 

I am looking for this material

15 NiCuMoNb 5/1.6368 (WB36)

This is the pipe used for power plants of 600 MW. I could not able to match its spec. with ASME. I require one meter spool piece of diameter more than 12’’ and thickness should be more than 40 mm for procedure qualification. I want to know following things.

 

1.      Source of material.

2.      What consumable to be used for GTAW/ SMAW/ SAW/FCAW.

3.      The parameters.

4.      PWHT heating cycle.

 

 

Regards

 

Ravinder Sharma

 

P  Please consider the environment before printing this e-mail       

 

 

 

 

 

 

 

 

 

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...