Hi pradeep  

It is client requirement.

On Sun, 7 Jun 2026, 08:12 pradip kumar Sil, <pradipsil@gmail.com> wrote:
 Appendix M is a non-mandatory appendix. Accordingly, its requirements cannot be enforced by the Client unless they are expressly stated in the contract or incorporated by reference in an applicable project document.  

On Thu, Jun 4, 2026 at 9:40 AM 'manish kulkarni' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Yes , it should be done in PQR as well . Convince customer for the approach




On Thursday, June 4, 2026, 11:31 AM, Nambirajan Avudaiappan <nambirajanavudaiappan@gmail.com> wrote:

This requirement is not applicable to PQR; it is applicable to WPQR.

For WPQR, can we measure the ferrite content using a ferritoscope during production in the shop, instead of performing the point count method?


Regards,


Nambirajan A


On Thu, 4 Jun 2026 at 11:05, atul jha <atulkrjha21@gmail.com> wrote:
The steps are :
1. Establish the PQR with extreme care as welding parameters will play crucial role in phase formation.
2. Do the ASTM 562 ( ferrite count by metallography) and ferritoscope( this is a portable machine and to be used on production weld principle is magnetic here ).
3. Welding on production weld shall be done by welding parameters established during PQR establishment.
4. With ferritoscope production weld phase can be measured.


On Thu, Jun 4, 2026, 9:13 AM Nambirajan Avudaiappan <nambirajanavudaiappan@gmail.com> wrote:

Dear Experts,

Good morning!

Has anyone performed ferrite–austenite phase evaluation for Duplex Stainless Steel (DSS)?

As per my understanding, this requirement has been incorporated in ASME Section IX under Non-Mandatory Appendix M (M-600). I would appreciate if you could share your experience, procedures followed, or any practical challenges faced during implementation.

Whether we can do with any machines without help of labratories

Looking forward to your valuable inputs.


image.png

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJuyB2W4yRfBs9N1zWWFd6EfNApA8u7-dqMYgr0HsXCkEDJVhA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAC1tTUKXVR-y0gQEXZ3ZFL8KzOvKeLzD8YF%2BU4dnTAW3sKVMYQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJuyB2UrLP9w33WxcDug_31wvpMUyPJyX%3DAFu-m59dHTbztyWQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/947735728.611840.1780558403591%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8nRS07PwqMjjmRyd1-g%2B_wY991M_KV8Ajs2FY4Y6acgFQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJuyB2UJVc-0CuV89mh%3D8Pmw_PjeoBf04DQWj2QjKjwWO8TryA%40mail.gmail.com.

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...