As per my opinion, If qualified 8mm plate min 5mm and Max 2T, weld metal -2t.
On Sat, 29 Mar, 2025, 08:30 Elavarasan Mech, <elavarasan1861994@gmail.com> wrote:
Please clarify belowAs per ASME SEC IX can we use 14mm plate machined to 8 mm plate for WPS & WQT qualification.please guide meRegardsELAVARASAN--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4ym4-UGqb6tprYjv66ifU7fan--MHmyUneojUPdVkv44Fg%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CABHGzEUreiX52fSUOKQoBekWdsxiYmtsDq_hwEoW8UfJ15h6aw%40mail.gmail.com.
Comments