Saturday, March 29, 2025

Re: [MW:35492] Buttering and overlay

Dear Mr Saini,

 major difference between weld with buttering and weld overlay are given below:
1. weld over lay 
     a. weld over lay have two types, one is hardface over lay another one is corosion resistance over lay 
    b. when we required harder surface with higher hardness than base materail - hardface over lay is being used
    c. when we required corrosion resistant surface in order avoid correcion- corrosion resistance over lay being used 
2. weld with butter 
    a. During dissimilar welding applaiction, buttering being used 
    b, when joining carbon steel to stainless steel, the carbon steel side buttering can be done before joining to SS materail 
    c. purpose of buttering to avoid the dilution effect & lossing of alloying  elements from weld metal 

you can refer AWS welding hand book for your further refernce.
     
 



Regards,
Sankaran.SP
Welding & Metallurgy expert
 


On Thursday 13 March, 2025 at 02:50:03 pm IST, Shahil Saini <sainishahil98@gmail.com> wrote:


Hello All,
Hope all are doing well,

Can anyone please explain the major difference between weld with buttering and weld overlay?

Regards & Thanks,
Shahilkumar Saini



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CALfBO_-cKMu1zr5m9f7nu35uH1%2BcoMdWRsyxqVPiAuqKKeay2Q%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...