Re: [MW:35490] Specimen Test location in PQR

Refer ASME Sec.IX  

1. QW-451                                  - Type & no. of tests for PQR
2. QW-462, Fig. 462.1 to 462.3  - Specimen sizes for each tests
3. Fig 463.1(a) to 463.1(d)         - Specimen location

Thanks & Regards

K.Dinesh 



On Thu, Mar 6, 2025 at 10:53 AM kumar sumit <kumarsumities@gmail.com> wrote:
Dear all 
               Can anyone Elaborate test specimens(Tensile, root,face/side bend and toughness test) location in PQR sample  with reference and also Size of specimen in which all test is covered.

Thanks

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CACCHnjWBosU1CDwrMprBs4AKcs26vsp%2B-pVrnbzsuxDpfj93YA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAG5OBYGSXBtXmyXMwok2JF5f3OFCKsUp9O7ZaCofAY0F7Dwk%3DQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...