Saturday, March 29, 2025

Re: [MW:35489] Specimen Test location in PQR

You have to refer ASME SEX IX , QW-462 For all desired details

On Thu, Mar 6, 2025 at 12:23 PM kumar sumit <kumarsumities@gmail.com> wrote:
Dear all 
               Can anyone Elaborate test specimens(Tensile, root,face/side bend and toughness test) location in PQR sample  with reference and also Size of specimen in which all test is covered.

Thanks

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CACCHnjWBosU1CDwrMprBs4AKcs26vsp%2B-pVrnbzsuxDpfj93YA%40mail.gmail.com.


--
Regards,
Rkumar Gohil
7874421813

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CACbJsYLwDr8sdMZSs8%2Bhv7a73VjaeBR20Td6k7ARMxWJ1Lxwhw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...