Re: [MW:35488] Re: 2411] Re: FW: 2390] Aluminium welding Data

In Aluminium welding, Cleaning Aluminium oxide, hydrated oxide to be cleaned mechanically & by ARC also.  Al2O3 has got melting temperature around 2400 deg celsius whereas Pure aluminium around 660deg celsius. Torch shall be water cooled to avoid high heat inturn, absorb hydrogen which is enemy to form pores. USE AC Square wave with Pure or Zirconiated Tungsten.
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015, ISO 3834, EN 15085, 
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Wed, Mar 19, 2025 at 10:25 PM James Bond <jamessbaand.786@gmail.com> wrote:
Dear Sir,

i have a job for aluminimum welding - 3mm sheet + 20 square tube welding.
this is my first time.

can u help me with this. - for aluminum welding.

how to do - how to prepare the surface - gas and welding parameters - pre requisities for aluminium welding.

kind regards,
k. vinodh kumar
hosur, tamil nadu, india
+91-9844035036

On Saturday, June 13, 2009 at 10:08:41 AM UTC+5:30 PB HEGDE wrote:

There is a vast difference in welding practices between Steel and aluminum welding.

i)Commonly Aluminum is welded by Tig and mig process

ii) For Tig process for more than 5mm thk AC tig is preffered with pure argon ,Pure tungsten is used. For AC tig DC suppressor is used for better performance, Preheating .is to be controlled properly. Weld pool is to be well protected from wind. Cleaning of filler metal before use is very essential. In case DC mode use electrode DC +ve to be used

iii)For mig Electrode  DC +ve to be used ,generally 1.2 dia wire on spool is used.

 

iv) For weld properties ,you will not be achieve the UTS as per base material. However 70% of base material strength is acceptable for weld and accordingly the base material thk is designed.

v)Some of the alloy require Aging or Heat treatment to improve the properties.

 

Aluminum welding is not that simple as steel welding as porosity is major problem you will face

 

Regards

 

Hegde P.B.

 

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of NILESH VARMA
Sent: Friday, June 12, 2009 9:17 AM
To: materials-welding@googlegroups.com
Subject: [MW:2411] Re: FW: 2390] Aluminium welding Data

 

Dear Hegde,
 Firstly thank you for the data given by you. For one of our jobs the material we are using is 6061 T651 as per AMS.
 Actually we wanted to know what are the common differences between steel & aluminium welding & also which are the problems commonly encountered while welding. As our objective is to provide the best product to our customer at low cost we are looking at exploring different fabrication techniques. Also it would obviously we clear to you that since Al is low weight material, the application demands extremely low weight & high strength application.

Regards,
Nilesh V.

On Thu, Jun 11, 2009 at 10:26 AM, PB HEGDE <hegde.pb@isgec.com> wrote:

Dear Nilesh

Attaching the welding and fabrication of aluminum But is there any specific Al alloy in your mind to know

 

Regards

 

Hegde p.B.

 

Subject: FW: 2390] Aluminium welding Data

 

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of NILESH VARMA
Sent: Wednesday, June 10, 2009 6:26 PM
To: materials-welding@googlegroups.com
Subject: [MW:2390] Aluminium welding Data

 

Dear friends,
 Can anybody help me out to find some really good aluminium welding technical data.

Regards
Nilesh V.

 

 



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/c64fca03-6599-479b-b342-86b985d87a7dn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eP%2BKh9rVhM08MtnxgXFcxnd%3DprBbCbqGmRSaJ6Z-zArcw%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...