Re: [MW:35475] ASME B31.3 minimum distance between two erlds

Pl refer IOGP S705 
Regards 



On Wednesday, March 5, 2025, 4:25 PM, Alan Hickey <alan.hickey@dornanprojects.com> wrote:

Folks,

This is always a very interesting topic, I have yet to see a clear answer.

Regards,
AlanHickey.

On Tue, 4 Mar 2025 at 17:07, Naina CPECC <nmeerane@gmail.com> wrote:
it should be 4t or 100mm whichever is greater valve  is  standard practice .Some international and client standard also define this parameter. This should be mentioned in your client specification , will vary depends on clients and service  

On Tuesday, March 4, 2025 at 4:51:51 PM UTC+3 Raviraj Gohil wrote:

Client specification Min. 50 mm Distance have to be maintained


On Tue, 4 Mar 2025, 18:59 Raviraj Gohil, <raviraj....@gmail.com> wrote:

With regards to Long seam you will get from ASME Sec VIII UW-9, But silent for Circ Seam However, Good Engineering Practices and One of client specification


On Thu, 27 Feb 2025, 14:54 Noman Ahmed, <nomi...@gmail.com> wrote:
Dear expert,
can somebody provide the latest CSWIP3.1 questions and answers with a new pattern.

Regards
NOMAN

On Wed, Feb 26, 2025 at 3:55 PM Matteo Meloni <matteom...@gmail.com> wrote:
Dear Experts

I'm involved on an activity of piping welding installation, and I didn't find on B31.3 any requirement of minimum distance between 2 welds.

do you have any info? also according ISO or other standard based on your experience

thanks for your support

Matteo 
IWI-C

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/d2233b5d-d28c-4e53-9e12-cbfecfc0b11fn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAM%2ByfweOirWgGkCu322YeeSmv8SVb_dbp5jsTJaEt7LR4p7Dtg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/419a169f-f63b-4015-8f8a-004c86e35671n%40googlegroups.com.

CONFIDENTIALITY NOTICE: This communication, and the information it contains, is (a) intended for the person(s) and/or organisation(s) to whom it is addressed and is for no other person(s) or organisation(s) and (b) may be confidential, legally privileged and protected by law, including law of copyright. Unauthorised use, copying, forwarding or disclosure of any of it may be unlawful. If you have received this communication in error, please contact us immediately by telephone to our head office number. We process personal data for the purposes explained in our privacy notice, which can be found here: https://www.dornan.ie/ privacy-policy/ . This notice also contains information about your rights.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAGFjgNH1xcokLxoXXc2kA9ngfL0wwEVEPJE8UVSj8SUboKrQyw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...