As per my understanding, the composition is typically as follows:

Copper (Cu): 88.0 - 90.0%

Nickel (Ni): 9.0 - 11.0%

Iron (Fe): 1.0 - 2.0%

Manganese (Mn): 0.5 - 1.0%

Zinc (Zn): ≤ 1.0%

Lead (Pb): ≤ 0.05%

Sulfur (S): ≤ 0.02%

Carbon (C): ≤ 0.05%

Phosphorus (P): ≤ 0.02%

Could you kindly confirm if this composition aligns with the latest specifications for SB466 C70600, or provide any additional insights regarding permissible variations?

BR, 

Deerendra. 


On Tue, 4 Mar, 2025, 18:05 Vishwas Keskar, <vvkeskar123@gmail.com> wrote:
Pl send chemical composition 
Sent from my iPhone

On 4 Mar 2025, at 12:23 PM, sujit kumar <sujitkumar19942@gmail.com> wrote:


Dear expert,

What filler wire We should use to weld SB466 C70600  to SB466 C70600 material.

What parameter should we use to weld that material. Specially when it will get crack??


Thanks and regards
Sujit

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAFonYWPKiRumE8qRDSg0wX1zAUZFCooUUJpKt8E7nQjqFwhPkw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/A4ACBB16-7E55-4871-A963-853F9C1B8F42%40gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAG0nF9F2s9cu%2BjpzCFjuL4NZ7o5p3mgQMoiH_xgnPBGgzSkjMQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...