Re: [MW:35464] Hot tapping between piping and pipeline

Hello,  

ASME B31.3 is not having any references clause for HOT welding procedure qualifications. 

Yes, the fitting design shall be designed inline to B31.3 for process piping and the field welding of the fitting on the live system shall be done as per API 1104 . 

Note : In case of fitting fabrication, let say in barred tee the weld joint between flange and sleeve , the shop welding can be carried out inline to ASME section IX. 

Regards,

Sudhakar K CEng MWeldI,IWE.

Welding & Metallurgical Engineer,

Email: sudhakarceng@gmail.com.



On Mon, 24 Feb 2025 at 11:24 AM, ali owead <aliawead1@gmail.com> wrote:
Dear Expert
we have hot tapping 
from process piping b31.3 design 
to cross country pipeline old pipe i think api 1104 design
WPS that need to folow  api 1104 or asme b31.3.
best regard.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/ffa0c881-23d8-4b3f-96d1-7337ed4ac1e1n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CABF8NYW_ULGEyE%3DuMTSik6kiBy_ctx0By4kYBuhruWOjNPFbdg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...