What is your plate material specification?
Material specification always refers to General specification requirements for plate size, dimensions, straightness as well as physical & mechanical properties.
For example if your material is SA 516 then you can find general requirements in SA 20 for all the tolerances and deviations.
Thanks & Regards
K.Dinesh
Metallurgist
On Thu, Sep 14, 2023 at 8:54āÆAM mohd helmi <mohdhelmi.hasmuni@gmail.com> wrote:
Dear Expert,--I have difficulties regarding material inspection. Now client reject my material inspection due to thinner plate not same with DO? for examples plate purchase 10mm now coming around 9.75mm, which code can I am refer to?
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHjDVH_%2B3Q%3DbxS5_3jTNHsFR9Xc8PznxNkdUgZzbFbY3JBuF6g%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG5OBYFSPi_WMa0BaZw6LYwXTVXB26BpTcjy%3Do_KP%2BGKPonU2Q%40mail.gmail.com.
Comments