Re: [MW:34544] Material Inspection Acceptance

Dear Helmy, 

If your plate is SA 36 then you can refer to SA6 where an under tolerance is provided which is 0.01 of an inch. 

However, I suggest you have a word with your design engineer & enquire about the minimum design thickness, if the design thickness is 9.75 mm then there is no need to worry about it & the plate can be accepted.

On Thu, 14 Sept 2023 at 07:54, mohd helmi <mohdhelmi.hasmuni@gmail.com> wrote:
Dear Expert,

I have difficulties regarding material inspection. Now client reject my material inspection due to thinner plate not same with DO? for examples plate purchase 10mm now coming around 9.75mm, which code can I am refer to? 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHjDVH_%2B3Q%3DbxS5_3jTNHsFR9Xc8PznxNkdUgZzbFbY3JBuF6g%40mail.gmail.com.

The information in this email and any associated files is confidential to Veolia Water Technologies (SASU) and/or any affiliate thereof and may be legally privileged. For the herein purposes, "affiliate" means any legal entity, partnership, joint venture, equity, company, including in particular any and all subsidiary which, directly or indirectly, controls Veolia Water Technologies (SASU) and/or is under the control thereof and/or is under the control of the ultimate parent company thereof, and "control" means the ability to directly or indirectly, direct the affairs of a third party by means of ownership, contract or otherwise. It may also contain information that is subject to copyright or constitutes a trade secret. It is intended solely for the named recipient. Access to this email by anyone else is unauthorized.

If you are not the intended recipient, please note that any use, disclosure, copying, distribution of this email or any action taken or omitted to be taken in reliance on its prohibited.

Warning: Although this email and any attachment thereto are believed to be free from viruses, it is the responsibility of the recipient to ensure that they are virus free. No responsibility whatsoever is accepted by Veolia for any loss or damage arising from their receipt or opening.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPus-A4dWOmnsysjzyT2XR%3DCwiU%3DyqoBCKqwYM16oqegqAGoyg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...