Re: [MW:34132] USE of PQR of 10.97mm GTAW+SMAW for new WPS GTAW process only

Ajay since you are preparing a WPS for GTAW only, Your WPS requires no changes, highlighted values are OK

Thanks & Regards

J.Gerald Jayakumar




On Thursday, 13 April, 2023 at 08:44:45 am IST, Ajay Kaipuram <ajaykdas144@gmail.com> wrote:


Thanks Mr. Jayakumar,

The impact test is No Applicable to our job.

Still, I have some doubts about preparing the WPS. Can you please review the area highlighted in the below screenshot? If changes are required, please let me know.

Screenshot 2023-04-12 123448.png

Thanks 

Ajay.



On Wednesday, April 12, 2023 at 6:29:05 AM UTC+3 james gerald wrote:
There are 2 thickness involved, Base metal (BM)Thickness and Weld metal (WM)thickness. Yes, you can prepare a separate WPS for GTAW from the PQR.

When Impact test is Applicable.

BM thickness Qualified,  minimum is 10.97mm so you cannot prepare a GTAW WPS.

When Impact test is not Applicable

BM thickness Qualified,  5mm to 7.0mm (though maximum is 21.94mm)


WM thickness Qualified is maximum 7mm

Thanks & Regards

J.Gerald Jayakumar



On Wednesday, 12 April, 2023 at 08:32:52 am IST, Ajay Kaipuram <ajayk...@gmail.com> wrote:


I have a PQR of 10.97mm Test coupon GTAW(3.5mm)+SMAW(7.47mm) in groove Joint, ASME Sec IX . 

Can I prepare a new WPS for GTAW only for the Job with thickness 5.08mm groove joints? If Yes, What thickness range need to be mentioned in the WPS? 5mm to 7mm is Ok?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/03b90f84-3657-431c-8002-d8122e47c3d6n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c5c8e34e-3aae-4746-a4b1-3f8b39370c2cn%40googlegroups.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .