On Tue, Aug 23, 2022 at 9:28 AM 'Neilash Kumar' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Yes before joining the olet to cladded pipe 

Step 1
Buttering on top of pipe face side wall  drilled location .

Step 2 
Grinding using same grade stainless wheel 

Step 3
Etiching using acids to see carbon replaced with stainless steel clad material 

Step 4 cladding and followed with NDT (UT and RT to see the full penetration joint .

Best Regards 
Neilash 



On Sun, Aug 21, 2022 at 11:52 AM, TANSON N
Dear All,
How is olet welded with claded pipe,is there any procedures to follow?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/aee9367e-e26e-418b-8255-6eea58c6128cn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/787077311.30738.1661189860697%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAyAb6PbPzu7MH7TV5i00o807QwEVXB5R_NKQ77jsSwQ3JbaQA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...