Saturday, September 24, 2022

Re: [MW:33505] Which filler wire can use?

We have already welded with ERCUNI filler wire using p34 to p34 WPS using GTAW process.

Does this welding is acceptable or not? If not, then suggest the welding requirement such as process, filler wire, procedure etc.

On Fri, Sep 23, 2022, 1:52 PM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
C38600 (Lead Brass) is not suitable for fusion welding, so u can do brazing using silver brazing rod

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Fri, Sep 23, 2022 at 3:39 PM Mubashir khan <mubashirkhan9642@gmail.com> wrote:
Dear experts,

Please give your valuable comments

 For CuNi C70610 and ASTM B62 C38600

For these base metal which filler wire we can use and why with reference thanks

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAALx7_LAOVwUcSkuRqHrA-wepN%3DsDgq%2BbZhwfsnpxaNnw5jaSQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePfN2Mxfi2a3vJUnkmF5v4CzXoE%3D70OawnUDkvdBA-HKw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAALx7_K8QJaO4DYVtHv%2BfM5PwUpvzhnsAa5EUZ5-vbqFqwRfEw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...