Re: [MW:33504] Which filler wire can use?

C38600 (Lead Brass) is not suitable for fusion welding, so u can do brazing using silver brazing rod

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Fri, Sep 23, 2022 at 3:39 PM Mubashir khan <mubashirkhan9642@gmail.com> wrote:
Dear experts,

Please give your valuable comments

 For CuNi C70610 and ASTM B62 C38600

For these base metal which filler wire we can use and why with reference thanks

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAALx7_LAOVwUcSkuRqHrA-wepN%3DsDgq%2BbZhwfsnpxaNnw5jaSQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePfN2Mxfi2a3vJUnkmF5v4CzXoE%3D70OawnUDkvdBA-HKw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...