Re: [MW:33497] E7018 Equivalent Filler Wire for SAW

F7A2EM12K

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Thu, Sep 22, 2022 at 2:27 PM Thota Kishore <krish.royal18@gmail.com> wrote:
Dear Experts,

Could anyone suggest the filler wire & suitable flux for SAW which shall be equivalent to E7018/SMAW.

Thanks in advance.
Regards,
Kishore 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALpPUFsEkoKqSdsHfwdPcTtjY4qGWaD%3DLW3vcyi0c-Yxo7x1%3Dw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOJSrU6_w1QcUiuiuJp%3D_aXkDmDBACxP0h2iHc5LdrJJQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...