Tuesday, September 20, 2022

Re: [MW:33488] Gas and welding rod compatibility

Dear Eda,
You can use Э-50А,УОНИИ13/55,РБУ-5,ЦУ-5 rod and kindly check the gas purity.

Regards,
Binit Kumar

On Sat, Sep 17, 2022 at 4:40 PM Eda Bekar <eddabekar@gmail.com> wrote:
Dear Experts,

The rod and gas we use in our project are СВ08Г2С (russian norm) and M21(%80 Ar + %20 CO2) . We have a lot of porosity and spatter problem. Could you give an advise better than this gas and rod combination?
Materials : C345-5,C255-4,09Г2С-15

Best Regards


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/937EC6BF-2A49-4929-8551-B6E4457E1006%40gmail.com.


--
BINIT KUMAR
+918717929495

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJ0ob9DRdtMBwy0YowZmvdXNcUKuwedDrDhjQuLsx8kAMbQ3AA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...