Thank you for your email sir.......I have a query sir  if we use ER-308H is there any issue with that...????

Best Regards.
Sujit Kumar

On Mon, 12 Sept 2022 at 11:38, Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
1, 347H
2.308
3. NiCr3
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Sun, Sep 11, 2022 at 11:45 AM sujit kumar <sujitkumar19942@gmail.com> wrote:
Dear all,

Greeting for the day.
 What filler wire we should use for the below material?

1.SA182 F304H TO SA213 TP 321.
2. SA213 TP304 TO SA182 F304H.
3. INCONEL 8800 TO SA213 TP304.





--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFonYWPKF6-Vsk%3DRUScM152Gj4MGrOvaRuoJDK%3D8F0srvrLiSw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMCrP97bxcRbv8UqV6ZXjgT_yvwqxxFC1gL1kLQt7Egwg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFonYWNCduDQJSvwug5jhXJ2_SkWyZSf%3DZyquh25stcyk0vptQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eM9LjSHidmO%2BfPRtnt3%2BpFDAa5WGJUZYpcX5889kME_cQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...