Increase more than the maximum heat input in the PQR.

On Mon, Sep 12, 2022, 2:07 PM williams p wilson <williamswilsonp@gmail.com> wrote:
Dear Experts,
Greetings!! 

Increase of Heat Input considered as an essential variable in SAW welding if impact test is required. Anybody can define the word "Increase" or how much 

Thank You & Regards
Williams P Wilson
+968-94600828
QA/QC Engineer
Please consider the environment before printing this message

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHBxnQ71_10vgqbJU6DNuratfCoqbH1uF%3Dz3Yrhj29-Gn9PMgA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAK-7o_PhAxFm%2BPjGh6t-FXfL9120QQM77jsBwjNo4X16D_fcFw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...