Wednesday, September 7, 2022

Re: [MW:33436] QW-407.2

1. QW407.2 is the supplementary essential variable.  This applicable when impact is required. Before carrying out the PQR, u have to calculate the what is the maximum base metal /weld metal thickness expected in Production, based on this, PQR should undergo minimum 80% time cycle of the production base metal , otherwise new pqr is to be done

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Mon, Sep 5, 2022 at 1:26 PM williams p wilson <williamswilsonp@gmail.com> wrote:
Dear Experts,

QW-407.2 is not applicable when an impact test is required, Please confirm.


Thank You & Regards
Williams P Wilson
QA/QC Engineer
Please consider the environment before printing this message

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHBxnQ5oT-m79w8dV_Bjeruvu5qfTPzyY4ouu9Uy%2BaZ5fd76mA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMRorvGf6w6VSuwqpGT-c-HFmT-u2rLHnCOVZYuu47%3DyQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...